Uddeholm Skolvar
FOR SUPERIOR HOT FORMING TOOLS
![uddeholm-skolvar-durability_600x400.png](/app/uploads/sites/216/productdb/api/uddeholm-skolvar-durability_600x400.png)
Reference Grade Hot Work (H13)
- Hot wear resistance 40%
- Plastic deformation resistance 40%
- Heat checking resistance 40%
- Premature cracking resistance 35%
Designations
Chemical composition
C | Si | Mn | Cr | Mo | V |
---|---|---|---|---|---|
0.70 | 0.20 | 0.45 | 5.00 | 2.25 | 1.60 |