Uddeholm Vanadis 30 SuperClean
HIGH SPEED STEEL WITH EXCELLENT COMPRESSIVE STRENGTH
Uddeholm Vanadis 30 SuperClean
- Abrasive wear resistance 75%
- Adhesive wear resistance 60%
- Ductility edge chipping resistance 40%
- Toughness gross cracking resistance 28%
Reference grade
- Abrasive wear resistance 55%
- Adhesive wear resistance 25%
- Ductility/edge chipping resistance 20%
- Toughness/gross cracking resistance 10%
Designations
-
Complex cut (CC)
Chemical composition
C | Cr | Mo | V | W | Co |
---|---|---|---|---|---|
1.28 | 4.20 | 5.00 | 3.10 | 6.40 | 8.50 |