Uddeholm Orvar 2 Microdized
EXCELLENT THROUGH-HARDENING PROPERTIES

Uddeholm Orvar 2 Microdized
- Hot wear resistance 40%
- Plastic deformation resistance 40%
- Heat checking resistance 40%
- Premature cracking resistance 35%
Reference Grade
- Hot wear resistance 40%
- Plastic deformation resistance 40%
- Heat checking resistance 40%
- Premature cracking resistance 35%
Designations
Chemical composition
C | Si | Mn | Cr | Mo | V |
---|---|---|---|---|---|
0.39 | 1.00 | 0.40 | 5.30 | 1.30 | 0.90 |