  • Abrasive wear resistance 75%
  • Adhesive wear resistance 60%
  • Ductility edge chipping resistance 40%
  • Toughness gross cracking resistance 28%

Reference Grade Hot Work (H13)

  • Hot wear resistance 55%
  • Plastic deformation resistance 25%
  • Heat checking resistance 20%
  • Premature cracking resistance 10%

Designations

Chemical composition

C Cr Mo V W Co
1.28 4.20 5.00 3.10 6.40 8.50